Devcon Plastic Steel Putty (A) vs Devcon Titanium Putty
Standard steel-filled putty vs titanium-reinforced premium putty.
// Key differences
- Compressive strength: ~57 MPa (Plastic Steel) vs ~105 MPa (Titanium).
- Dry heat: up to +121°C vs up to +177°C.
Choose Devcon Plastic Steel Putty (A) for:
Everyday repairs of cracks, holes and housings.
Choose Devcon Titanium Putty for:
Worn shafts, bearing seats, high-load and hot parts.
Full specification comparison
| Parameter | Devcon Plastic Steel Putty (A) | Devcon Titanium Putty |
|---|---|---|
| Manufacturer | ITW Devcon | ITW Devcon |
| Category | Metal Repair Composites | Metal Repair Composites |
| Temperature range | -40°C … +121°C | -40°C … +177°C |
| Standards / approvals | MIL-PRF-24176 | REACH |
| Chemistry | Steel-filled epoxy | Titanium-reinforced epoxy |
| Operating temperature | Dry: up to +121°C / Wet: up to +49°C | Dry: up to +177°C / Wet: up to +65°C |
| Compressive strength | 57 MPa | 105 MPa |
| Working time | 45 min | 40 min |
| Functional cure | 16 h | 16 h |
| Specification | MIL-PRF-24176 | REACH |
| TDS & quote | TDS & quote |
Data compiled from manufacturer data sheets — confirm critical values with the official TDS.
More comparisons
- → Loctite 243 vs Loctite 270
- → Loctite 401 vs Loctite 406
- → Loctite 577 vs Loctite 574
- → Loctite 518 vs DOWSIL 736 Heat Resistant Sealant (ex Dow Corning 736)
- → 3M Novec 7100 vs Opteon SF79
- → 3M Novec 7100 vs 3M Novec 7200
- → 3M Novec 7300 vs Opteon 2P50
- → Krytox GPL 205 vs Krytox GPL 226
- → Fomblin Y LVAC 25/6 vs Fomblin RT 15
- → Belzona 1111 (Super Metal) vs Belzona 1321 (Ceramic S-Metal)
- → Belzona 1111 (Super Metal) vs Devcon Plastic Steel Putty (A)
- → Klübersynth UH1 14-151 vs DOWSIL 111 Valve Lubricant & Sealant (ex Dow Corning 111)
- → BitCool BC-888 vs Shell Immersion Cooling Fluid S5 LX